    Donna, as a vendor who probably deals with more silver than you and
    I would ever see in a lifetime, yours probably just doesn't have the
    time or manpower to check silver strands to make sure he's getting
    silver. Like the rest of us, he is given a statement (either verbal
    or written) saying that what he's buying is sterling silver. If he
    gets too many complaints, then he'll go to the source and find out
    what the culprit is. Generally, when a supplier says it's silver, it
    is. 

    Now as far as the round beads that are being affected by your
    magnet, did you have these for a long time? Could you have purchased
    silver plate at the time not knowing there was a difference between
    SS & SP? In the past two years, I've learned many such lessons and
    now have a good bit of SP that I just don't use because at the time I
    bought it, I didn't know any better. 

    Good luck on your hunt! 

Betty
www.thecyrusco.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project