From: Lee Einer Date: Wed Sep 15 20:55:43 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== OK, two patinas- First, Baldwin's Patina from Reactive Metal Studios will color the copper a nut brown while leaving the silver as is. Second, You can flux the piece, heat it with the torch to annealing temp, let it cool for a minute or so and then quench in cold water. The copper will turn burgundy or cherry red. This is a deep patina, and I have successfully polished such pieces with Zam without losing it. Haven't tried it on mokume gane, but I have tried this with silver solder inlay on copper, and with silver overlay on copper, and the results were satisfactory. Lee Einer Dos Manos Jewelry http://www.dosmanosjewelry.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project