    Okay, on this thread... I have a strange question... 

    I have created some sterling pendants where I solder a dome onto
    another sheet.  As a hole is needed for the gases to escape, I
    usually create a heart in the back of the piece to make it more
    attractive, to compliment the piece. 

    I use steel shot to polish,(could not afford stainless when I bought
    it, but it has held up for 3 years already) . However, because of
    the size of the 'heart' in the back, I am getting  the long striaght
    shot pieces stuck in my dome.  So, how can I keep that from occurring
    without having to make the 'heart' size no longer look complimentary
    to the piece? Do I need to purchase different shot that won't fall
    in? 

    Any help would be appreciated.  I truly appreciate the inspiration I
    receive on Orchid...  (and thank you Metals-Edge!) 

Heidi Peters
HP Designs

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project