Sharron,

    It's always hard to give decent advice without being able to see
    your design (wish there were an easy way of posting images here),
    but it sounds to me like the best solution would be to solder your
    bezel onto flat sheet and cut it out (making it a separate bezel
    cup). Get your textured shape as flat as possible, place your bezel
    cup where you want it to go, and scribe a line up tight to the edge.
    Cut out the area defined by the scribe (along the inside of the
    scribe line) and check to see that the bezel fits well into the
    cutout shape. Solder it in from the back to prevent solder flow on
    the textured area. 

    A similar issue was covered in a recent project in Lapidary Journal:
    something like "Mystic Turquoise Pendant" or "Mystic Turquoise
    Bezel". Definitely mystic, anyway. It was a good step-by-step that
    described several such handy techniques. 

Good luck with your piece!

Jessee Smith
www.silverspotstudio.com

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project