    Prevention is worth a pound of cure. There are a variety of sources
    for "silica gel" which is a "desiccant" that works ...if the tools
    are stored inside a drawer or tool box... to dehumidify air and
    prevent "corrosion" which contribute to (rusting) steel. That
    "corrosion" ...(rust) which is iron oxide... the chemical Fe2O3.,
    read all about it at 

    http://science.howstuffworks.com/question445.htm. 

    There are probably many sources; my quick web search found several
    products at this URL http://www.air-tites.com/ATsupplies.htm Also,
    searching Orchid for the term desiccant returned some results. Often
    we store and use a variety of chemicals; some of which may be
    "oxidizers". For those up for a little experimenting on testing your
    chemicals for their pH levels (are your chemicals "acids" or
    "bases"?) ...visit http://www.howstuffworks.com/experiment1.htm 

Regards, 
Mark 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project