========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Here are a couple of ways to tell when Kum Boo is hot enough. I, allso, use a steel plate to heat on. If you sand a small area clean before heating, when it turns blue, you've reached heat. Sound handy? Well, I just learned a much more convenient method from our own Elaine Luther. Keep a toothpick or bamboo skewer on hand. When touching it to the workpiece (or was it the piece of metal for heating on? Elaine?) causes it to turn brown or black, or give off a tiny puff of smoke, it is hot enough. I have tried this, and found it very convenient and effective. I touched it to the workpiece, since I was working on a series of pieces that had, oddly enough, a piece of tubing on the back, and therefore didn't lie flat. No hole, didn't think to hang it over the edge. It worked great. HTH! --Noel ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project