>         as it all stayed immersed in the soapy water, it never rusted 

Hi Noel.

    I have read lots of postings over the past two years about shot of
    various composition, and methods of storing and cleaning it.I  have
    come to the conclusion that either I buy new stainless or as I have
    been advised, rustless shot, or I put up with the problems of
    cleaning the shot each time I use it. 

    I have tried all sorts of tips  and whatever I do, if I don't want
    to dry the shot each time I use it, I have  black gungy shot under
    greeny black gungy liquid in the barrel and I must clean it by
    tumbling it in Coke and fairy liquid (the best combination for me.)
    It only takes about 30 mins to clean, with one or two  changes of
    liquid and I now accept that this is the best I can do for the
    moment.  However, I have just read the posting about adding washing
    soda to the mix, so another experiment looms. 

Ruth in the UK.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project