From: Karen Bahr Date: Thu Aug 12 10:02:34 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Trevor You could use copper or brass tubing instead as they won't contaminate the same and especially with copper you can still reuse your filings in water casting. That is what I do. Mix filing that I have gone over with a magnet a couple of times with fresh casting grain (I use fine to offset the extra copper that may be in my filings) and melt and pour into a large bucket of cold water. My students love seeing ways of reusing scrap and the funky shapes and cups are great for decorating. Karen Bahr "the Rocklady" (rocklady AT nucleus.com) K.I.S. Creations May your gems always sparkle. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project