From: Trevor F Date: Tue Aug 03 09:51:53 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > ... May I suggest that razor blades as such were probably not > meant. Hello John, Sorry to contradict JB but I believe that Charles --Mr. Lewton-Brain-- did in fact mean razor _blades_. You can find the process and procedure in his "Cheap Thrills in the Toolshop", p.34. I think it's also online at Ganoksin ... yup, http://ganoksin.com/borisat/nenam/jumpring.htm 'bout halfway down the page. Razor saws are great but it's definitely a razor blade that is used in the technique Charles describes. That said I've tried the process and on my couple attempts made a horrible mess of an otherwise useful wire coil. My guess is that it's only intended for small and/or very small gauge wire and even then it's going to take you a bit of practice to get it right. I moved on to other techniques but have never forgotten the image of zipping off dozens of jump rings at a go. Cheers, Trevor F. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project