>         do you all sand the edges of your jump rings after sawing? 

Hello Jocelyn,

    FWIW I've found that if you use a fairly fine blade in your saw, say
    4/0 or 5/0, and make a point of doing as smooth a cut as you can you
    end up with rings that require no further dressing before soldering. 

    It helps immensely if the coil is very snug on it's core while you do
    the sawing. Wrapping on an aluminium tube, locking the ends down in
    slots cut in the ends of the tube and then taping the coil snugly with
    an end-to-end overlapping wrap of masking or painter's tape is
    sufficient to accomplish this.  Every once in a while you'll need to
    start with a new piece of aluminium tubing 'cause your ends get sawed
    up but the stuff is cheap and effective so it's no biggie. 

    The aluminium tubing seems to work better than the traditional wooden
    doweling because you can wrap, tape and saw a tighter coil, at least
    that's what I've experienced. 

Cheers, 
Trevor F.

____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________

  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project