========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Isabel, Stainless steel is wonderful for making the "nests" to hold your work while soldering. I like the 24 gauge since it does hold up for several soldering operations. If you are doing a larger item, I like to get steel wire, dead soft, from the hardware store. It is about 19 gauge and holds the pieces just fine. It is called bailing or banding wire and is found in the building department of the local home improvement store. It comes in a small dispenser pack and is less than $3.00 as I remember it. Not all stores carry it, but if you hunt around you are sure to find it. It is a product used to bail hay in case someone wants to know what it is used for. With the stainless wire, it can go in the pickle. The iron or steel wire cannot so do not be tempted. Beth Katz Unique Solutions Inc. http://www.myuniquesolutions.com) Paste and Powder Solder for Jewelers and Metalsmiths ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project