From: kgoeller Date: Wed Jun 02 19:57:22 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Brian, Whenever I heat silver (sterling or fine) to annealing temperatures, I do it in a regular "room" atmosphere using a torch. You didn't say whether you're using sterling or fine silver, so I'm assuming sterling. However, any time you heat sterling silver to annealing temps, you will get a change in the surface structure that will "cloud" it (bringing the fine silver toward the surface by depleting the copper in the alloy) -- and likely outright oxidation. Pickling following annealing is always required, in my experience. I can't think of any case where annealing would be the final finishing step for a piece; you'll always be pickling and doing final polishing after annealing and shaping. Am I missing something in what you're trying to do? Karen Goeller kgoeller AT nolimitations.com www.nolimitations.com ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project