    The very best thing that I have found is a product called Stop-Flo.
    It is an amazing product in that it will stop the solder from
    flowing, yet is quite easy to remove one you have completed the
    heating of the piece.  You simply place the piece in water to soften
    the Stop-Flo and it will allow you to take it off with nothing more
    than a soft (used) toothbrush. The liquid has to be applied with a
    brush and does dry quickly but it is well worth the price.  It never
    leaves a trace once you have removed it and it really is very easy to
    remove, unlike yellow ochre or white out (that is a true disaster in
    my book). It is available from the Mine Shaft in Ft. Lauderdale
    954-917-7821.  I am looking into making this one of the products to
    carry, it is that good. One aside for the yellow ochre, you can mix
    the powder with olive oil to make it more easy to remove than when
    mixed with water.  It still cannot shine a candle to the Stop-Flo

    Beth Katz Paste and Powder Solder for Jewelers
    http://www.myuniquesolutions.com



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project