| Re: [Orchid] Large silver cups casting | ||
|
[Thread Prev]
[Message Prev]
[Date Index]
[Thread Index]
[Message Next]
[Thread Next]
From: James Binnion Date: Thu Apr 29 23:24:38 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Mark, One thing I would try is lowering your flask temperature. With castings that large and thick as the ones you describe you should be able to cast at about 900F-1000F this will make for better castings. You ideally want as cool a flask as will fill. You may need to do some experiments to verify what temp is best. A lower flask temperature will produce better surface finish and less porosity. For your bubbles you may want to try hot water investing. This has been used by casters at similar altitudes to Denver with some success. Check out http://www.preciousmetalswest.com/ they have a description of the process on their website. There are some folks who don't like this technique but it is one solution to bubble problems at high altitude casting shops. Jim Binnion James Binnion Metal Arts Phone (360) 756-6550 Toll Free (877) 408 7287 Fax (360) 756-2160 http://www.mokume-gane.com jbin AT mokume-gane.com Member of the Better Business Bureau ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project