    I have just made a necklace using more than a couple of thousand jump
    rings which I made by winding the wire around a knitting needle of
    the required diameter then cutting the rings by hand. 

    I make my rings the same way since I don't really do enough volume
    to justify buying a jumpringer, I use a setup that was suggested to
    me by one of the exceptional instructors at George Brown (thank you
    Ellen). Essentially it is a plastic cutting board clamped to the edge
    of my bench with various holes drilled in it, a couple of steel
    plates and some leather to guide the wire at the edge. Feed the wire
    though to the needle inserted in the hole, clamp the wire to the
    needle with a pair of vice grips and twist away. I get a perfect coil
    in a few seconds. Total cost about $7.00 and you can get all the
    parts at Canadian Tire or local US equivalent. If anyone wants a jpeg
    of the setup, you can e-mail me off line. Cheers, Stephanie Morton


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project