========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Back again Anyone interested in ferric chloride etching should search "Keith Howard" and words like "non-toxic etching". Keith is a printmakers who seems to know a lot about ferric chloride. One idea I got from him is to use a liquid acrylic floor wax as a "hard ground". He suggests adding india ink (I've added acrylic paint) so you can see it against the scratched metal. It's good for doing 'intaglio' type etching - i.e. fine lines. But you can also paint it on with a brush. One thing that seems somewhat critical for success with this is to sheet on the wax and let the metal sit vertically (so most wax drips off leaving a fine layer of wax) and scratch through the wax with a scriber after about 20 minutes. If it gets too dry the edges seem to lift off - so the 20 minutes seems important. Someone mentioned not using Sharpie pens. I agree. I use Staedtler Lumocolour permanent markers in the transparent colours (red, blue etc - NOT black). By the way, I am scheduled to teach a married metal and etching course at Metalwerx in Boston this summer, if anyone would like to learn more. I also have notes on my website on etching with ferric chloride. It's a technique I love. Once you try it, you get hooked. It's also a great technique to teach to beginners as the results are always impressive. ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project