    To who-ever was asking - Komelia Okum of Washington DC gives classes
    in this and Kumboo.  We just finished a weekend class with her in
    Seattle. (Komeliaokim AT aol.com) 

    For the Damascene - sand one side of the steel well.  2) using a V
    chisel cut lines in rows from left to right up the piece to cover it.
     Then turn the piece by l80 deg and chisel across the first
    chiselling. 

    3) Then chisel diagonally both ways - think of a plus sign with an X
    over it and you get the chiselling directions.  This gives tooth to
    the steel and one can then inlay .025mm silver or gold wire and gold
    or silver foil cut into designs.  Use a rivetting hammer to do this
    and do not hammer too hard. 

    4) When piece is done dip in black solution with a few drops of
    amonia added. (Can't remember the name of the black stuff at this
    time).  Watch it carefully because you get the blues coming first and
    if left in longer it goes very black. 

    5)  Tumble it to set all. 

    Good Luck   Glen Paris 

    PS Komelia is a fantastic teacher and her class was priceless. 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project