From: Jeff Demand Date: Mon Mar 29 22:32:55 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Karen, Use Hard solder for the best colour match, fewer nasty alloys to tarnish. Also do not depend on binding wire to hold your joint closed, at soldering temperatures it anneals and stretches. A much better method is to bend the shank to get a spring closure. Still annealing concerns, as the shank gets hot you loose some of the spring action but still much better than trying to force the joint closed with a frail soft wire. A rolled thin piece of solder larger than the join can be inserted into the sprung joint. Wasteful, but it does insure enough solder. And of course LOTS of practice. Jeff ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project