========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Lee, I told ya so! I have had great success using the wire mesh on charcol blocks (or tufa or mag or whatever). What torch are you using? I usually use my acetylene/air with a very large tip when doing such projects. The secret in this case is torch and flame control. Make sure you have an extra heavy layer of Prip's flux on the thing as there is going to be lots of heat needed. Don't heat the back plate too fast and, while you must get the entire plate hot, don't try to get the entire backplate up to full solder heat at once - only work on one section at a time. Be sure the solder is well drenched in Batterns or what ever self pickeling flux to preclude it from oxidizing. I have done very large and heavy belt buckles this way with no problems. Some I have to heat 4 or 5 times to sweat solder on various layers. Good luck and cheers, Don at the Charles Belle Studio in SOFL where simple elegance IS fine jewelry! dcdietz AT comcast.net ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project