    While working at the 3M products/demonstration tables at the recent
    SNAG Conference in St. Petersburg I talked with many attendees about
    their use of the 3M Radial Bristle Discs. One problem we discovered
    is quite common. Many artists and students were using one disc at
    time mounted on their mandrel. These discs are intended to be stacked
    together to make a high performance brush. I would suggest for the
    9/16" and 3/4" size that stacking six discs together will make the
    best performing brush. For the 1" size stacking at least three discs
    together is best. Also, when using these high performance brushes a
    light touch on the surface of your work piece will bring you the most
    satisfactory results and the longest life. The majority of the
    artists who had been stacking the discs love using these little
    bristle brushes. 3M is proud to support SNAG ... see you in Cleveland
    next year !!! 

    Rick Pihl - Product Development Specialist - 3M Abrasive Systems
    Division 


R i c k   P i h l
3M  Abrasive  Systems  Division
3M Center,   Bldg 251-3A-05
St. Paul,  MN    55144-1000

Office : 651-733-0824
FAX :    651-733-6376
Email :  rmpihl1 AT mmm.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project