    Have you considered using Zam instead of rouge? It's cleaner to work
    with and gets good results. 

    One bench trick that I have found with the use of fabuluster, on
    gold, and your flex shaft is to use it with the stiff bristle brushes
    and a little Wintergreen oil or liquid bur life.  This makes a kind
    of gray mess, at first but once you get through the sludge it creates
    all of the sudden you have a really great shine pop through.  I
    learned this from a really great stone setter from South America some
    30+ years ago.  He did all his bright cutting or pave and when he was
    done he hit it with fabuluster and Wintergreen.  It was a beautiful
    thing to watch. 

    I agree that for general use as a polish it is ok but does not give
    the best polish.  There are many other products which will do better.
    With the stiff brushes and for certain applications, it is hard to
    beat. 

Have a great day,
Phillip Scott G.G.
Technical Support & Sales


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project