    Michael, I used a lot of copper 12 gauge wire when I was starting
    out. It was the kind encased in a tube of plastic. To remove the
    casing, I used a moderately sharp pocket knife, and pulled the wire
    down between the knife and the edge of my work table. It worked very
    well. Have you started forging the wire yet? The hammer marks from
    forging can cover or obliterate any nicks that you might cause with
    the knife, and moving the metal through forging gives it a lot more
    interesting form than just plain round wire. Loosen up, and have fun
    with your recycled material! By the way, if you move on to hard
    soldering, copper is an excellent trainer, since any flooding of
    excess solder really shows up. It will teach you to be very neat, so
    that if you try silver or gold, you will know how to create a tidy
    joint. Copper solders well with silver solders. Best wishes for your
    work! -- M'lou Brubaker, Jeweler Goodland, MN   www.craftswomen.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project