Hello all,

    My question is a consequence of leaping before I looked. I have made
    an enameled large pendant with two holes for jump rings. Once the
    piece was "finished" I added the jump rings and with a little
    manipulation and a whole lot of luck I was able to solder the ends
    together. My intention was to put a silk cord through the rings, but
    after having done so, the piece still unfinished. The piece itself
    seems to be OK because I have received compliments on it. Hence I
    have decided to add an element at the top so that the cord goes
    through it. The element in turn is then attached to the pendant. I
    have done this with other pendants and seemed to create something
    that worked. 

    My worry/concern is that if the ends of the jump ring are not on a
    surface, I won't be able to solder them together because of heat
    loss from radiation. 

    Do you have any suggestions? Also other design solutions are
    welcomed. 

    Finally would a drawing, followed up by a mock up, say in paper,
    reveal my design flaw? 

    Why such a large piece? Because one afternoon walking home from work
    I got to chatting with a large women after complementing her on her
    gorgeous coat. We got to talking and after a while she
    commented/complained to me that very little jewelry is made for the
    large women, at least here in Victoria. I got me thinking and
    acting. 

    Sorry for the essay, (a man of many words when just a few will do). 

David


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project