    Hi bill and everyone Namaste 

    If I remember correctly this stain may have been there before the
    lady had bought the ring. Only in such an indistinguishable intensity
    that neither me nor the lady have noticed it! But looking back, I do
    have the feeling that it has started before she bought the ring. 

    There are no suppliers of alloyed gold in this part of India [as far
    as I know...] There's this wonderful family on one of the jewellers
    streets that I buy my gold from, they usually mix the alloy for me as
    they have a large charcoal furnace and the experience of a family
    line. They do my refining as well. 

    It is possible that at times, the refining process they do, may not
    remove some? impurities [this has happened before, resulting with an
    alloy which was nearly unworkable.] 

    What can I do now to remove this stain from the ring in such a way
    that it will not re-appear ? 

    In the past I did thought it works like a miniature spring of oozing
    black stuff... and it  would eventually exhaust itself. Will the heat
    of soldering temp. help ? 

	The Pickle ?
	Neutralizing ?
	The ultrasonic ?
	Caustic soda ?
	Other kind of chemical ?

    Please help me with this one. Love & Light akash 

www.akashjewels.com
contact AT akashjewels.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project