    Dear Kathy, My favorite media is the Clean Cut media. Based on the
    description of your pieces having medium detail I would mix cone and
    pyramid together in equal proportions of both for the medium cut
    (339-408) cone, (339-441) pyramid and the same for the fine cut,
    (339-410) cone, (339-443) pyramid. 

>      And I'm also thinking of adding some stainless steel pins to my
>     stainless shot mix. Which size pins are more effective: 9/32" or
>     1/2"? 

    As for the stainless steel pins, I don't think it matters unless you
    have very fine detail you need the pins to get into. Remember that
    the pins may "ping" your smooth areas on your work. The pins are
    designed so the points get into tight nooks and crannies (sp). They
    are not designed for smooth surface areas. 

    e-mail me off list or call me at 1-800-545-6566 if you wish. 

    I Hope this helps. 

Regards,
Thackeray Taylor
Rio Grande Technical Support


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project