    Invisible setting has posed many problems as it was readily embraced
    by manufacturers that really had no clue. Some pieces that I have
    seen are accidents waiting to happen. This as particularly true of
    the no-wall pieces that have come onto the market. Most manufacturers
    ask that you send any work, including sizing back to them. Many state
    that they will not work on any piece that has been worked on
    previously by someone else. That said, I recently came across an
    advertiser in Modern Jeweler magazine (March 2004) that bills itself
    in bold headline "INVISIBLE EXPERTS". "Specializing in invisible set
    diamond jewelry" I have not used this service and cannot recommend
    them, but I thought that I would pass this information along. The
    name of the company is Signature Jewelry. 877-8-EXPERT.,
    213-624-6026. They are at 617 South Olive St. Suite 302, 
    Los Angeles, CA 90014. 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project