    I can think of only 2 reasons a Superfit would not stay closed. 
    Adjustment is first.  By properly adjusting the closing tension by
    reshaping the bottom section, it should stay closed.  If it is too
    loose, or otherwise misaligned, it will open.  The other problem is
    if the top section is too light to hold the tension.  This would
    result from letting the original ring to be the entire structural
    element on the top, which in some cases is incorrect.  IMHO, these
    are one of the best of the arthritic shanks, at least the one I like
    to recommend most often.  I haven't had any trouble with one yet,
    though some have required creative installation to maintain
    structural integrity and therefore proper fit and operation.  If all
    else fails, contact the company and see if they have any ideas (I'm
    assuming you don't have the installation instructions in front of
    you). http://www.superfit.net 

Jim in NC mountains, where the ski season is done and spring is trying
really hard to arrive.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project