    invisible settings, very expensive to repair! here's a story for
    this method! 

    I lady came to me and told me one diamond fell out of her, 6 stone
    wide, total eternity ring. It had over 150 Princess stones. $25,000
    wholesale cost mounting! 

    So in Toronto, we have one manufacturer with the name of "Mirage"
    who deals in this style of setting stones. This fellow said "Gerry,
    if I have to replace one stone, I have to remove all the stones AROUND
    the missing stone, re-cut by Laser a new stone to fit, and likening a
    jig-saw puzzle re-arrange the remaining stone to re-fit again. His
    cost to me was $475.00 CDN. As many remaining stones were loose he
    would not at all guarantee the others in the mount, nor would he
    attempt to tighten any other stones. He said that all of these
    stones should be well cared for. No one should abuse jewellery with
    invisible set stones. As all of the invisible stones are wax-set,
    manual setting is not done and to set just one stone is left to the
    mavens in this style of setting. He also said that jewellery like
    this must re-checked for security one a year.....Gerry! 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project