From: Noel Yovovich Date: Tue Mar 09 23:11:45 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Yes, you can change media, if you *clean very very thoroughly* between media,. especially when going from coarser to finer. There are many to choose from, and I had a lot of fun using aluminum oxide (I think-- or was it corrundum?) on glass to etch deeply into it and do 3D things. I didn't pursue it, but it clearly had potential. I've always meant to try that technique on, say, rose quartz, but never got around to it (so far). Quartz is pretty hard, so it might not work, but should on maybe turquoise or other "soft" stone... NOT malachite, that would be too toxic! Anyway, have fun! By the way, anything resilient and rubbery will work well as a resist: rubber cement, Elmer's glue, watercolor frisket, masking tape, paint marker, stickers, electrical tape (which is stretchy and will conform to a domed surface) plus, of course, the tapes made for the purpose such as "buttercut" which is expensive and not so easy to find. Yikes! I've given you an earful you didn't ask for. Pity my poor students! Noel ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project