From: Dave Date: Mon Mar 08 21:01:11 2004 |
||
========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Hi Elaine, > What are the difference btw sandblasting and beadblasting? The difference between the two are basically the media & as a result the type of finish produced. Sand blasting is a system of using clean, sharp sand or other media like garnet, silicon carbide, aluminum oxide etc. propelled by a high pressure air stream. The stream of air & media is directed at a surface to abrade it for cleaning or to texture it. Typically, if the finish is important, the media used is graded by grit size to give the desired finish. Bead blasting typically uses glass beads instead of the other media. It is also graded by size. The big difference between the two types of media is one of hardness & grain shape. The glass media is lighter, softer, rounder & has fewer sharp edges. For a given air pressure, it leaves less of an impression on the surface being blasted. Both types of media can use the same basic machinery for application. Dave ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project