>         I do think that the oxy-hydrogen torch that the original poster
>     asked about is a "water torch", which manufactures oxygen and
>     hydrogen from water only in the amount needed at 

    Yes, that's what I thought too. They are a small self contained unit
    which require distilled water and some liguid flux that is added, if
    I remember right. I worked at a custom jewelry store where my boss
    had a Hydroflux Welder on his bench. He used it for soldering
    platinum. I soldered platinum at my bench too but I used natural gas
    and oxygen rather than the oxy-hydrogen. 

    What I remember is that it had a relatively small, very hot, flame.
    He often had trouble keeping the torch lit. It seemed to me to have
    very little range of use. I have just now looked one up in the Rio
    Grande catolog. Hydroflux units are still almost $1000 and there is
    a picture of the type of flame they produce. The ad says it can
    solder or fuse platimun up to 22 grams and can solder a heavy size
    13 class ring. I never felt that my boss' unit could do that but
    perhaps the new units are better. There's another one called Hot
    Flame. I've never seen it in action. It is $1690. 

    I'm sticking with my oxygen/propane torch but it would still be
    interesting to hear if anyone in the Orchid group is regularly using
    a "water torch." 

Jennifer
Highland Goldsmith


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project