========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== When creating and repairing inlay pieces I use my flat lapidary to first grind flat (180 grit diamond) then work the piece with progressively finer laps (340/600/1200). Once I've finished with the 1200 it takes just a light touch on the buffing wheel with Zam and/or Fabuluster to get a nice finish. Too much polishing on the buffing wheel does start removing the epoxy as it is the softer material. To do this manually after you finish with the file start polishing the stone on progressively finer grades of wet/dry sandpaper and water on a flat surface (polished granite floor tiles work well). You can get up to 600 grit wet/dry sandpaper at your local hardware store or home center. Auto parts stores carry wet/dry sandpaper in finer grits. Hope this helps. Rick Copeland Silversmith and Lapidary Artisan Colorado Springs, Colorado http://home.covad.net/~rcopeland/ ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2008, The Ganoksin
Project