    Natural gas is safer to use than propane (in most areas of the
    country it's illegal to store propane tanks indoors).  And natural
    gas is cleaner to use than acetylene.  But in many locations,
    natural gas pressure is not high enough to run a casting torch.  

    There are options however ... from torches specially designed to run
    at high oxygen pressure and low natural gas pressure ... to natural
    gas boosters which are a safe and fire-marshall-approved method of
    increasing the natural gas pressure supplied to your shop. 

    So don't give up on natural gas just because the pressure you're
    supplied is low. Check with your tool supplier for options that can
    make it work for you. 

    Best Regards, Elaine Corwin VP Technical Services www.gesswein.com
    Gesswein Co. Inc. The Right Tools 1-800-544-2043 x287


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project