========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Kevin, Natural gas will be suitable for most of your needs with the possible exception of casting and even that if you get a high pressure line or compressor. When you set up your system make sure to have a check valve placed on the natural gas line between the torch and the gas supply so that any blockage in the torch nozzle will not allow oxygen to enter the natural gas line because the oxygen will more often the not be at a higher pressure than the gas line and can force its way back down the line if the torch tip becomes blocked for any reason, that can cause a fire or worse. For safety reasons you normally want the gas and oxygen pressure to be the same so that this can't happen but with natural gas you will have a low pressure line and most oxy regulators can not be set to operate reliably at as low a pressure as the gas line. -- Jim Binnion James Binnion Metal Arts Phone (360) 756-6550 Toll Free (877) 408 7287 Fax (360) 756-2160 http://www.mokume-gane.com jbin AT mokume-gane.com Member of the Better Business Bureau ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2007, The Ganoksin
Project