========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== Kevin, I have used a Meco Midget torch with natural gas from a standard house type gas line (normal house pressure is 11" W.C. which is about 1/2 psi) when I was at the Revere Academy it works fine for soldering small jewelry size items but is not enough volume of gas to work on large items or to cast. Some business do get high pressure natural gas delivery but you would need to have a new line brought in and this would involve permits, trenching and plumbers and $ so using natural gas to cast is not normally an option. There are natural gas compressors that take in gas at normal line pressure and compress it to about 60 psi and store it in a small tank these systems are in the low thousands of dollars price range and used most often by folks who can't for either legal or insurance reasons have high pressure or high volume gas tanks on site. -- Jim Binnion James Binnion Metal Arts Phone (360) 756-6550 Toll Free (877) 408 7287 Fax (360) 756-2160 http://www.mokume-gane.com jbin AT mokume-gane.com Member of the Better Business Bureau ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project