    Hello Janet, I use the 2mm diameter flex-shaft polishing pins from
    Rio (p.393 in the 2004 Tools and Equipment catalogue) for finishing
    hard-to-access tiny spaces. I have a mandrel for each abrasive grade
    so that I don't have to fiddle with changing pins. The pins may be
    easily shaped by running the tips against abrasive paper. I
    especially like them for polishing chasing tools or the depressions
    of beading tools. 

    The only time I've had trouble with the mandrel's collet not holding
    the pins in has been when more than about 5mm of the polishing pin
    protrudes from the collet after it has been tightened down. Unless
    you've been leaving too much of the polishing pin exposed, you may
    have gotten a defective collet/mandrel with your kit. If you did have
    the bad luck to receive a "lemon" collet with your kit, I have found
    Rio Grande to be very good about refunds or replacements. 

Best Wishes,
Anne M. Kelly


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project