From: David Tranter
Date: Wed Feb 25 21:12:57 2004
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    One way that I have found to be successful is the  following: 

    1. Decide on the outside diameter of the donut and make a 1/2 sphere
    conforming to this dimension.  Make sure you drill a small hole in
    the centre of the disc before dombing.  

    2. Place finished sphere, domb facing up in a pitch bowl. 

    3. At location of predrilled hole, proceed to deform metal with
    various sized ball punches (small to large) down into the pitch until
    desired shape has been achieved but making sure to anneal adequately
    during process.  

    4. Turn donut over in pitch bowl and work from back if necessary. 

    Hope you find this explanation adequate and look forward to reading
    other suggestions.  Have a good one from David Tranter in sunny Cape 
    Town, South Africa.  aurum AT worldonline.co.za.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project