    The following has just gone out with the JPM email newsheet 

    .. and I'd love to hear of any personal experiences using laser
    welding on antique pieces. 

    LASER WELD REPAIRS TO ANTIQUE JEWELLERY. 

    Laser welding is now commonplace in jewellery manufacturing and
    repair. The technique, which affects only microscopic areas and uses
    very localised heat, is increasingly being used to make almost
    imperceptible repairs on antique gold jewellery. Those involved with
    antique jewellery in any capacity should recognise the characteristic
    weld marks (for examples on a Victorian locket hinge see
    http://www.jpm-international.com/JPMGallery/Laserweldjpg.html ). A
    use of laser welding in the restoration of a seventeenth century
    enamelled gold and silver monstrance has recently been published (C.
    Innocenti, G. Pieri, M. Yanagishita, R. Pini, S. Siano and A. Zanini.
    Application of laser welding to the restoration of the ostensory of
    the martyr St. Ignatius from Palermo. Journal of Cultural Heritage,
    4, no. Supplement 1 (2003) 362-366 - first reported at a conference
    on Lasers in the Conservation of Artworks (LACONA) held in Paris in
    2001). The authors believe that this is first application of laser
    welding in the conservation of a work of art. The 'non-reversibility'
    of the joining process will attract some criticism from within the
    conservation community. 

    By the way if any of you would like a copy of the whole newssheet by
    email (topics range from recently excavated ancient jewellery to  De
    Beers talk's with the US Justice Department) just send an email to
    info AT jpm-international.com and put 'sample' in the subject line. 
    The newsheet goes out two or three times a month and it's free to
    sign up. 

Jack Ogden
International Jewellery & Precious Metal Network (JPM)


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project