    There are definitely some resins and epoxies that put off too much
    heat for fragile materials; but have you ever seen the resin with
    scorpions embedded, or the resin with dandilion "fluff ball" seed
    stems within?  Lots of people embed fairly fragile items (like
    photographs) in epoxies. 

    "Noel suggested that

>              With resin enamel, new non-heat-resistant materials can
>     be incorporated, for example. There is, in fact, quite a lot of
>     heat given off in the chemical processes involved , and I would
>     hate for anyone to accidently ruin a precious object. It is, of
>     course, nothing like as hot as kiln-fired vitreous enamels, but
>     this would be little consolation in such circumstances. You need
>     also to consider the potential corrosiveness of the resin; if it
>     takes the skin off your fingers, and the lining off your lungs,
>     then it's a fair bet that it is not going to do much for fine wood

    Stevie, it actually sounds like you are using fiberglass resins,
    which are flammable and toxic.  There are some much milder resins
    and epoxies out there. 

--Terri


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project