    I'd just like to make two points on the "resin vs enamel" issue.    

    1) There is precedent far calling things other than
    glass-fired-onto-metal enamel. Go to the paint department of any
    hardware store! 

    2) And more important: My personal opinion is that resin "enamels"
    should not be looked at as a imitation vitreous enamel any more than
    PMC should be regarded as imitation casting. Yes, the materials can
    be used that way, but each is, in fact, a material/process on its
    own. As such, each offers creative opportunities that did not exist
    before. With resin enamel, new non-heat-resistant materials can be
    incorporated, for example. The colors can be inlaid into wood (or
    vice versa), found objects, all kinds of things that vitreous cannot
    touch. I'm sure this is not even the tip of the iceberg.            
    
    Of course no one should mislead others about the nature/identity of
    materials. But we will all have more opportunities for creativity if
    we try to keep our minds open. 

--Noël



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project