    Will, I am working with impressions made into pink sheet wax. But I
    do not use my rolling mill to do it, I use a screw press . I spray
    the wax surface with silicone spray that is meant for wax release in
    a rubber mold, put a fresh green leaf vein side down on it, and
    enclose it in a sandwich of the waxed (or perhaps plastic-coated)
    paper that comes in the pink wax box to separate the wax sheets in
    shipment. Experiment with how much pressure to use, as too much
    squishing is bad. I also use the screw press to get impressions of
    the plastic photo etchings made with Model Master (see Rio Grande) 3M
    materials. The impressed wax sheets can then be cut with scissors,
    welded with wax tools, and made into more 3-D designs for casting. I
    have been having a lot of fun with it. I think it will work just
    fine with paper, too, as long as you can get the paper to peel off of
    the wax after pressing it. My green leaves create some juice that
    sometimes helps release the leaf residue , though they sometimes get
    stuck if they are too dry. Using the silicone spray is the key to
    having this work at all, as I found through much experimentation. I
    think your results would be much more controllable with a screw press
    than with a rolling mill, because of how a mill will tend to push the
    wax ahead of itself instead of just impressing it from the top. Know
    what I mean? I was going to keep this technique to myself for a
    while, but I just cannot resist the power of Orchid's sharing energy!
    - M'lou Brubaker www.craftswomen.com 



____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project