Hi Alma,

    Try Bryant Labs in Berkeley, CA   800-367-3141 

    This is where I get all my patination and etching chemicals.  I
    order Ferric Nitrate in 5lb jars.  Make sure you keep the lid closed
    very tight, as it will suck up water like a sponge.  I throw one of
    those packets of silica dessicants that I find in packages of candy. 

    Use one cup of ferric nitrate to three cups of water.  You want the
    solution to look like strong tea.  Etch the same as ferric chloride. 

    When you are through with the solution, pour it into some kitty
    litter and bag it up.  Easier to recycle that way. 

    One tip, use DISTILLED water.  Also, make sure that your silver is
    VERY clean.  Try to touch it only by the edges after cleaning. 

Good luck!

Karen Christians
M E T A L W E R X
50 Guinan St.
Waltham, MA  02451
Ph: 781/891-3854
Fx: 781/891-3857
www.metalwerx.com
email: karen AT metalwerx.com


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2007, The Ganoksin Project