From: Geosoul Arts
Date: Fri Jan 16 06:33:57 2004
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    Hi Pam.  I can't offer you much advice on the silver work part of
    your question but being that I am a dichroic glass cabochon
    manufacturer I can offer you a bit of advice on working with the sea
    glass.  If you put the glass in the kiln, it's not going to look like
    sea glass anymore.  I would think that the whole charm and character
    of sea glass is that it has been matte finished and worn smooth by
    being tumbled through the sea.  If you melt the glass, it will become
    nothing more than just another piece of glass.  Even if the glass
    doesn't actually melt, the temperature you bring it up to might be
    enough to change how it looks by slightly slumping it, changing the
    shape slightly, or even altering the matte finish.  I imagine that
    your customer might be very unhappy about a change to the look of
    her glass.  Just a thought, I hope it helps.  Good luck with your
    project! 

Sincerely,
Nancy Stinnett, Owner
Geosoul Arts
www.geosoul.com
(702) 436-7685


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project