    Hi all, I would really appreciate some input regarding the following
    challenge: i am putting together an anklet and matching bracelet in
    sterling silver for someone.  the chain is made of silver curved bars
    linked with closed jump rings.  she wants sapphire-blue Swarovski
    heart crystals to dangle from each jump ring.  I have the crystals,
    and they are beautiful, but when i experimented with different gauges
    of silver wire i noticed the crystal scratched a bit around the hole
    (they have a very small hole right in the "v" part of the heart for
    stringing).  Can anyone give me input as to how to avoid this
    scratching?  will using a very fine gauge silver wire take care of
    the problem?  are there any other creative ways to dangle these
    crystals from the closed jump rings?  also, if i do use silver wire,
    i'd like to solder the loop closed, so i'm assuming i need kook jool
    or something like that -- correct?  is crystal very sensitive to
    heat? Thanks in advance! Lois


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project