========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== A word about citric acid pickle-- When I ran out of standard pickle, I mixed up some citric. I got impatient with it, and threw in the tiny bit of Rio pickle I still had. I can't give measurements, but I would guess that it amounts to maybe 10-20%, if each were mixed with water and combined. It seems to me that this has produced a very effective, much safer but still fast pickle. I'm still using that batch, so I have not had occasion to try to duplicate it. Does anyone know any reason that this is a bad idea? It seems to me (with no scientific basis) that the addition made the pickle just about as fast as just the Rio pickle, despite being mostly citric. Has anyone else tried this? --Noël ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project