    Hi Janet,

    I made a two colour moebius strip during the xmas break, white and
    yellow gold, with the join between the two colours cut as a wavy line
    - started with a strip of 1 mm thick yellow, cut wavy bands of .3 mm
    white to fit approx. half the  width of the yellow, soldered one each
    side of the yellow, put through the rolling mill, then twisted and
    joined to make the finished strip - worked very well, so I made it
    into a pendant for my partner- he loves it. I think with what you
    want to do, etching might be an option, but have you considered using
    something coloured, such as resin? Then you could make a plain
    moebius, and pait the resin on - this might work well, or maybe using
    a textured strip from wax, sorry if I'm being a bit obvious with
    these suggestions, but I am getting very enthusiastic about all of
    these possibilities :-) 

Christine in Sth Australia.


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Blogs
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2009, The Ganoksin Project