========[ Invite a Friend - http://www.ganoksin.com/invite.htm ]======== > Speaking about safety, health and pickles, please understand > that the fumes of sodium bisulphate are *cancerogenic*. A note that to my knowledge the fumes are corrosive (ie steel tools rust) but are not carcinogenic. The mist of a sulfuric acid containing solution is however carcinogenic which is one of the reasons you should not quench hot metals into a sodium bisulfate pickle-it produces a mist of minute droplets. Charles Charles Lewton-Brain/Brain Press Box 1624, Ste M, Calgary, Alberta, T2P 2L7, Canada Tel: 403-263-3955 Fax: 403-283-9053 Email: brainnet AT telus.net ____________________________________________________________________ T h e O r c h i d L i s t Open Electronic Forum for Jewelry Manufacturing Methods and Procedures ____________________________________________________________________ Orchid FAQ: ~ http://www.ganoksin.com/orchid/faq.htm Orchid Archives: ~ http://www.ganoksin.com/orchid/archive Orchid Galleries: ~ http://www.ganoksin.com/orchid/gallery.htm Invite a Friend: ~ http://www.ganoksin.com/invite.htm ____________________________________________________________________ Tips From The Jeweler's Bench - Article Archive ~ http://www.ganoksin.com/borisat/tip_sear.htm The Jeweler's Selected Bibliography List ~ http://www.ganoksin.com/jewelry-books Buy Orchid Jewelry: ~ http://www.ganoksin.com/shop ____________________________________________________________________ -Unsubscribe: -Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank ____________________________________________________________________ |
||
| Navigate: | ||
|
||
| Orchid Resources: | ||
|
Join & Post Invite a friend to join Orchid F.A.Q Galleries BenchExchange Orchid Blogs Orchid Message Archives [Subject Index] [Date Index] Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!
|
||
© Copyright 1996 - 2009, The Ganoksin
Project