Karen,

    Jay's reply sounds like a good arrangement. 

    I had started with a friend showing me the basics of making a
    straight and beveled herringbone chain out of silver from melting my
    own material through rolling, drawing wire, annealing, etc.  The
    first ring I sized was my own...He walked away from me and said to
    call him if I needed help.  It took me 1 hour to size that ring. 
    Most of that time was spent wondering what to do. 

    The point is you learn by doing.  I got that tone from Jay's
    response too. I wouldn't pay anyone to be an apprentice...Why would
    they teach you enough to become independant?  They should pay you for
    the work you are able to do for them albeit at trade rates. 

    Since you want to keep your full time job, my suggestion would be to
    find a partime job with a local small jeweler. One who works the
    bench themselves.(You'll find out pretty quickly if they are capable)
     This way you can get some experience in small doses, help out in the
    store, and in return ask for exposure to the bench. It will also give
    you access to help should you need it for projects you undertake on
    your own.  Everyone needs help they can rely on when things get busy
    both on the floor and in the shop.  Think of it as symbiotic
    relationship. 

Good luck,

Mark


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project