From: Tim Goldstein
Date: Fri Jan 09 00:15:40 2004
 
     
========[ Invite a Friend - http://www.ganoksin.com/invite.htm  ]========


    The jump ringer is just not suitable to cut Ti rings. The blade RPM
    is drastically too high so that you will burn the blades in Ti. Ray
    Grossman makes a special unit that incorporates a motor which turns
    the blade at 200 rpm which is much more in line for the proper
    cutting speed for Ti or steel. Even at that speed you would likely
    want a wated mixed cutting oil to keep the blade from overheating and
    dulling. If you are determined to try with the standard jumpringer
    you will want a solid carbide blade, but in the thickness required
    they are EXTREMELY fragile and any sideload will snap them instantly.
    

Tim 
A2Z Metalsmith Supply Inc 
5151 S Federal Blvd Unit I-9 
Littleton CO 80123 
720 283-7200 
www.A2ZMetalsmithSupply.com 


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project