    Here are a few tips: 

    1.  I purchased "Diamond Setting: An Introductory Procedure," a
    video by Robert Wooding.  For me it was a quantum leap in my
    technique.  I have not been disappointed in any of the videos I have
    purchased from Rio Grande. 

    2.  Bee's wax softened between the fingers for handling small stones 

    3.  The Allset tool is remarkable 

    4.  The Bench Mate ring clamp allows both hands free to work. 

    5.  Curved jaw pliers allow you to see your work better as you bend
    prongs over the bezel facets 

    6..I use cast or stamped mountings but I solder 22 gauge wire to the
    outside. This adds strength and gives you enough material to work
    with. 

    Good Luck...This is not an easy venture on which to start out. 

Howard Woods
In the beautiful foothills near Eagle Idaho


____________________________________________________________________
T h e   O r c h i d   L i s t
Open Electronic Forum for Jewelry Manufacturing Methods and Procedures
____________________________________________________________________
Orchid FAQ:
~ http://www.ganoksin.com/orchid/faq.htm
Orchid Archives:
~ http://www.ganoksin.com/orchid/archive
Orchid Galleries:
~ http://www.ganoksin.com/orchid/gallery.htm
Invite a Friend:
~ http://www.ganoksin.com/invite.htm
____________________________________________________________________
Tips From The Jeweler's Bench - Article Archive
~ http://www.ganoksin.com/borisat/tip_sear.htm
The Jeweler's Selected Bibliography List
~ http://www.ganoksin.com/jewelry-books
Buy Orchid Jewelry:
~ http://www.ganoksin.com/shop
____________________________________________________________________
-Unsubscribe:
-Email: orchid-request AT ganoksin.com Body=unsubscribe subject=blank
____________________________________________________________________


  Click to Visit  
     
  Navigate:  
   
  Orchid Resources:  
   Join & Post
 Invite a friend to join Orchid
 F.A.Q
 Galleries
 BenchExchange
 Orchid Message Archives [Subject Index] [Date Index]

Ganoksin now offers a number of ways for you to stay on top of the latest from Orchid!

  1. My Yahoo - Do you have a My Yahoo page? If so, you can easily read the latest Orchid posts on your personalized page by adding this feed:Add Orchid to My Yahoo!
  2. Add Orchid to myGoogle Add to my Google
  3. Read Orchid with NewsGator and Microsoft Outlook Add Orchid to Your  NewsGator
Support Orchid! - If you believe in what we're doing, you can help!

 
     
     

© Copyright 1996 - 2008, The Ganoksin Project